Description: Beveled copper panels typically have a significant depth for bold heavy-shadowed effects. In order to provide the rigidity required, the minimum recommended thickness for copper is 20 ounce half-hard temper alloy.
Panels are typically limited to 10 foot lengths. Transverse seams are 6", minimum, lap joints. The joints must be staggered on successive runs to reduce the build-up of multiple layers of copper at one point, which would make it difficult to fold the horizontal joints. This is particularly important since beveled panels use fairly rigid copper material.
Note: Panel profile, thickness and lengths must be reviewed per structural considerations.
Substrate: Continuous nailable substrate.
Fastening Method: Cleats screwed to substrate.
12.3A. Typical Section
A single lock seam is used in the horizontal joint between runs. Cleats, spaced at 16" on center, are used to fasten the panels to the substrate.
![DWG icon](../../../../../images/global/icons/dwg.png)
12.3B. Typical Axonometric
This detail shows an overall view of a beveled panel wall system. The deep panels provide strong horizontal shadow lines. The transverse seams should be staggered, as shown.
![DWG icon](../../../../../images/global/icons/dwg.png)
12.3C. Inside Corner
Copper flashing is laid over wood blocking in the corner to close the gaps at the ends of the panels. The flashing extends a minimum of 4" under the panels, and is held by cleats at 12" on center.
![DWG icon](../../../../../images/global/icons/dwg.png)
12.3D. Outside Corner
The ends of the panels in this condition are closed by copper flashing. The flashing extends a minimum of 4" under the siding and a minimum of 1" over it. Wood blocking and trim is used to finish the corner. An alternate detail is shown in Detail D in Wall Cladding - Profiled Panels.
![DWG icon](../../../../../images/global/icons/dwg.png)